onolithic Options: Clear,Tinted, Low Iron,Pyrolytic low-E,Reflective, Acid etched,Patterned, Silk Screen,Digitally Printed
Architectural Products Standards:: GB/T11614-2009, GB/T15763.2-2009,EN 12150-1,ASTM-C1048,ASTM-C1036
Exterior Applications: Glass Facade/Spandrel, Spider Glazing-Glass Fin/Mullion ,Greenhouse/Conservatory ,Glass Canopy/Balustrade/Handrail
Interior Applications: Frameless Shower Door,Glass Partition ,Glass Table Tops, Glass Furniture
Architectural Toughened glass spontaneous breakage (about 3‰) without warning due to the expansion of nickle sulfide inclusions(NiS) present within float glass, it is inherent potential risks of toughened glass.
Heat soaking test is good solution to test the toughened glass and reduce the probability of self-exploded and ensure quality,the shattering proof process is used for high requirement projects.
Production capability:
Glass | Thickness | Min Size | Max Size |
Heat Soaked Glass | 2.5-19mm | 300*300mm | 10000*3300mm |